Application number | Title of the application | Filing Date | Status |
---|
Array
(
[id] => 2447862
[patent_doc_number] => 04765834
[patent_country] => US
[patent_kind] => NA
[patent_issue_date] => 1988-08-23
[patent_title] => 'Process for the recovery of metal values'
[patent_app_type] => 1
[patent_app_number] => 6/871747
[patent_app_country] => US
[patent_app_date] => 1986-06-09
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 0
[patent_figures_cnt] => 0
[patent_no_of_words] => 9629
[patent_no_of_claims] => 10
[patent_no_of_ind_claims] => 1
[patent_words_short_claim] => 122
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => patent
[pdf_file] => patents/04/765/04765834.pdf
[firstpage_image] =>[orig_patent_app_number] => 871747
[rel_patent_id] =>[rel_patent_doc_number] =>) 06/871747 | Process for the recovery of metal values | Jun 8, 1986 | Issued |
06/868029 | HYDROMETALLURGICAL ARSENOPYRITE PROCESS | May 28, 1986 | Abandoned |
06/863031 | COMPOSITION AND USE OF THE COMPOSITION FOR THE EXTRACTION OF METALS FROM AQUEOUS SOLUTIONS | May 13, 1986 | Abandoned |
Array
(
[id] => 2336769
[patent_doc_number] => 04668483
[patent_country] => US
[patent_kind] => NA
[patent_issue_date] => 1987-05-26
[patent_title] => 'Process for recovery of chromium'
[patent_app_type] => 1
[patent_app_number] => 6/861683
[patent_app_country] => US
[patent_app_date] => 1986-05-12
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 1
[patent_figures_cnt] => 1
[patent_no_of_words] => 1921
[patent_no_of_claims] => 9
[patent_no_of_ind_claims] => 1
[patent_words_short_claim] => 286
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => patent
[pdf_file] => patents/04/668/04668483.pdf
[firstpage_image] =>[orig_patent_app_number] => 861683
[rel_patent_id] =>[rel_patent_doc_number] =>) 06/861683 | Process for recovery of chromium | May 11, 1986 | Issued |
Array
(
[id] => 2286968
[patent_doc_number] => 04678647
[patent_country] => US
[patent_kind] => NA
[patent_issue_date] => 1987-07-07
[patent_title] => 'Process for the recovery of gallium and germanium from coal fly ash'
[patent_app_type] => 1
[patent_app_number] => 6/861985
[patent_app_country] => US
[patent_app_date] => 1986-05-12
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 0
[patent_figures_cnt] => 0
[patent_no_of_words] => 2039
[patent_no_of_claims] => 11
[patent_no_of_ind_claims] => 1
[patent_words_short_claim] => 114
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => patent
[pdf_file] => patents/04/678/04678647.pdf
[firstpage_image] =>[orig_patent_app_number] => 861985
[rel_patent_id] =>[rel_patent_doc_number] =>) 06/861985 | Process for the recovery of gallium and germanium from coal fly ash | May 11, 1986 | Issued |
Array
(
[id] => 2361393
[patent_doc_number] => 04666685
[patent_country] => US
[patent_kind] => NA
[patent_issue_date] => 1987-05-19
[patent_title] => 'Selective extraction of molybdenum and vanadium from spent catalysts by oxidative leaching with sodium aluminate and caustic'
[patent_app_type] => 1
[patent_app_number] => 6/861689
[patent_app_country] => US
[patent_app_date] => 1986-05-09
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 0
[patent_figures_cnt] => 0
[patent_no_of_words] => 5220
[patent_no_of_claims] => 9
[patent_no_of_ind_claims] => 2
[patent_words_short_claim] => 189
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => patent
[pdf_file] => patents/04/666/04666685.pdf
[firstpage_image] =>[orig_patent_app_number] => 861689
[rel_patent_id] =>[rel_patent_doc_number] =>) 06/861689 | Selective extraction of molybdenum and vanadium from spent catalysts by oxidative leaching with sodium aluminate and caustic | May 8, 1986 | Issued |
Array
(
[id] => 2319344
[patent_doc_number] => 04670229
[patent_country] => US
[patent_kind] => NA
[patent_issue_date] => 1987-06-02
[patent_title] => 'Cyclic process for recovering metal values and alumina from spent catalysts'
[patent_app_type] => 1
[patent_app_number] => 6/861690
[patent_app_country] => US
[patent_app_date] => 1986-05-09
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 1
[patent_figures_cnt] => 1
[patent_no_of_words] => 4459
[patent_no_of_claims] => 12
[patent_no_of_ind_claims] => 2
[patent_words_short_claim] => 209
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => patent
[pdf_file] => patents/04/670/04670229.pdf
[firstpage_image] =>[orig_patent_app_number] => 861690
[rel_patent_id] =>[rel_patent_doc_number] =>) 06/861690 | Cyclic process for recovering metal values and alumina from spent catalysts | May 8, 1986 | Issued |
Array
(
[id] => 2316867
[patent_doc_number] => 04670052
[patent_country] => US
[patent_kind] => NA
[patent_issue_date] => 1987-06-02
[patent_title] => 'Process for the recovery of gold from a precious metal bearing sludge concentrate'
[patent_app_type] => 1
[patent_app_number] => 6/860433
[patent_app_country] => US
[patent_app_date] => 1986-05-07
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 1
[patent_figures_cnt] => 1
[patent_no_of_words] => 2332
[patent_no_of_claims] => 11
[patent_no_of_ind_claims] => 1
[patent_words_short_claim] => 100
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => patent
[pdf_file] => patents/04/670/04670052.pdf
[firstpage_image] =>[orig_patent_app_number] => 860433
[rel_patent_id] =>[rel_patent_doc_number] =>) 06/860433 | Process for the recovery of gold from a precious metal bearing sludge concentrate | May 6, 1986 | Issued |
Array
(
[id] => 2439956
[patent_doc_number] => 04740243
[patent_country] => US
[patent_kind] => NA
[patent_issue_date] => 1988-04-26
[patent_title] => 'Metal value recovery from metal sulfide containing ores'
[patent_app_type] => 1
[patent_app_number] => 6/858369
[patent_app_country] => US
[patent_app_date] => 1986-04-30
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 0
[patent_figures_cnt] => 0
[patent_no_of_words] => 6198
[patent_no_of_claims] => 40
[patent_no_of_ind_claims] => 2
[patent_words_short_claim] => 109
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => patent
[pdf_file] => patents/04/740/04740243.pdf
[firstpage_image] =>[orig_patent_app_number] => 858369
[rel_patent_id] =>[rel_patent_doc_number] =>) 06/858369 | Metal value recovery from metal sulfide containing ores | Apr 29, 1986 | Issued |
Array
(
[id] => 2377760
[patent_doc_number] => 04752332
[patent_country] => US
[patent_kind] => NA
[patent_issue_date] => 1988-06-21
[patent_title] => 'Treating manganese-containing ores with a metal sulfide'
[patent_app_type] => 1
[patent_app_number] => 6/858056
[patent_app_country] => US
[patent_app_date] => 1986-04-30
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 0
[patent_figures_cnt] => 0
[patent_no_of_words] => 7158
[patent_no_of_claims] => 41
[patent_no_of_ind_claims] => 2
[patent_words_short_claim] => 80
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => patent
[pdf_file] => patents/04/752/04752332.pdf
[firstpage_image] =>[orig_patent_app_number] => 858056
[rel_patent_id] =>[rel_patent_doc_number] =>) 06/858056 | Treating manganese-containing ores with a metal sulfide | Apr 29, 1986 | Issued |
Array
(
[id] => 2295395
[patent_doc_number] => 04681628
[patent_country] => US
[patent_kind] => NA
[patent_issue_date] => 1987-07-21
[patent_title] => 'Gold Recovery processes'
[patent_app_type] => 1
[patent_app_number] => 6/855406
[patent_app_country] => US
[patent_app_date] => 1986-04-24
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 0
[patent_figures_cnt] => 0
[patent_no_of_words] => 2972
[patent_no_of_claims] => 11
[patent_no_of_ind_claims] => 1
[patent_words_short_claim] => 130
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => patent
[pdf_file] => patents/04/681/04681628.pdf
[firstpage_image] =>[orig_patent_app_number] => 855406
[rel_patent_id] =>[rel_patent_doc_number] =>) 06/855406 | Gold Recovery processes | Apr 23, 1986 | Issued |
Array
(
[id] => 2486352
[patent_doc_number] => 04828809
[patent_country] => US
[patent_kind] => NA
[patent_issue_date] => 1989-05-09
[patent_title] => 'Separation of nickel from copper in autoclave'
[patent_app_type] => 1
[patent_app_number] => 6/855897
[patent_app_country] => US
[patent_app_date] => 1986-04-24
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 8
[patent_figures_cnt] => 9
[patent_no_of_words] => 5342
[patent_no_of_claims] => 24
[patent_no_of_ind_claims] => 6
[patent_words_short_claim] => 152
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => patent
[pdf_file] => patents/04/828/04828809.pdf
[firstpage_image] =>[orig_patent_app_number] => 855897
[rel_patent_id] =>[rel_patent_doc_number] =>) 06/855897 | Separation of nickel from copper in autoclave | Apr 23, 1986 | Issued |
Array
(
[id] => 2400485
[patent_doc_number] => RE032612
[patent_country] => US
[patent_kind] => NA
[patent_issue_date] => 1988-02-23
[patent_title] => 'Formation of tungsten monocarbide from a molten tungstate-halide phase by gas sparging'
[patent_app_type] => 2
[patent_app_number] => 6/855284
[patent_app_country] => US
[patent_app_date] => 1986-04-24
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 0
[patent_figures_cnt] => 0
[patent_no_of_words] => 2956
[patent_no_of_claims] => 11
[patent_no_of_ind_claims] => 2
[patent_words_short_claim] => 104
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => patent
[pdf_file] => patents/RE/032/RE032612.pdf
[firstpage_image] =>[orig_patent_app_number] => 855284
[rel_patent_id] =>[rel_patent_doc_number] =>) 06/855284 | Formation of tungsten monocarbide from a molten tungstate-halide phase by gas sparging | Apr 23, 1986 | Issued |
06/855196 | USE OF AN AQUEOUS SWOLLEN MACROMOLECULE-CONTAINING SYSTEM AS WATER FOR FIRE FIGHTING | Apr 22, 1986 | Abandoned |
Array
(
[id] => 2581127
[patent_doc_number] => 04891061
[patent_country] => US
[patent_kind] => NA
[patent_issue_date] => 1990-01-02
[patent_title] => 'Process for treating speiss'
[patent_app_type] => 1
[patent_app_number] => 6/854237
[patent_app_country] => US
[patent_app_date] => 1986-04-21
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 1
[patent_figures_cnt] => 1
[patent_no_of_words] => 2436
[patent_no_of_claims] => 7
[patent_no_of_ind_claims] => 2
[patent_words_short_claim] => 124
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => patent
[pdf_file] => patents/04/891/04891061.pdf
[firstpage_image] =>[orig_patent_app_number] => 854237
[rel_patent_id] =>[rel_patent_doc_number] =>) 06/854237 | Process for treating speiss | Apr 20, 1986 | Issued |
Array
(
[id] => 2441088
[patent_doc_number] => 04751070
[patent_country] => US
[patent_kind] => NA
[patent_issue_date] => 1988-06-14
[patent_title] => 'Low temperature synthesis'
[patent_app_type] => 1
[patent_app_number] => 6/852470
[patent_app_country] => US
[patent_app_date] => 1986-04-15
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 0
[patent_figures_cnt] => 0
[patent_no_of_words] => 2131
[patent_no_of_claims] => 24
[patent_no_of_ind_claims] => 4
[patent_words_short_claim] => 92
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => patent
[pdf_file] => patents/04/751/04751070.pdf
[firstpage_image] =>[orig_patent_app_number] => 852470
[rel_patent_id] =>[rel_patent_doc_number] =>) 06/852470 | Low temperature synthesis | Apr 14, 1986 | Issued |
06/850484 | METHOD OF EXTRACTING A PRECIOUS METAL FROM AN ORE | Apr 10, 1986 | Abandoned |
06/850637 | HIGH PURITY LITHIUM OXIDE PROCESS | Apr 10, 1986 | Abandoned |
Array
(
[id] => 2417332
[patent_doc_number] => 04734270
[patent_country] => US
[patent_kind] => NA
[patent_issue_date] => 1988-03-29
[patent_title] => 'Sulfide treatment to inhibit mercury adsorption onto activated carbon in carbon-in-pulp gold recovery circuits'
[patent_app_type] => 1
[patent_app_number] => 6/850677
[patent_app_country] => US
[patent_app_date] => 1986-04-11
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 1
[patent_figures_cnt] => 1
[patent_no_of_words] => 5030
[patent_no_of_claims] => 22
[patent_no_of_ind_claims] => 4
[patent_words_short_claim] => 116
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => patent
[pdf_file] => patents/04/734/04734270.pdf
[firstpage_image] =>[orig_patent_app_number] => 850677
[rel_patent_id] =>[rel_patent_doc_number] =>) 06/850677 | Sulfide treatment to inhibit mercury adsorption onto activated carbon in carbon-in-pulp gold recovery circuits | Apr 10, 1986 | Issued |
Array
(
[id] => 2295430
[patent_doc_number] => 04696810
[patent_country] => US
[patent_kind] => NA
[patent_issue_date] => 1987-09-29
[patent_title] => 'Wet process for the production of a readily sinterable powder material of perovskite or its solid solution'
[patent_app_type] => 1
[patent_app_number] => 6/847148
[patent_app_country] => US
[patent_app_date] => 1986-04-02
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 0
[patent_figures_cnt] => 0
[patent_no_of_words] => 4758
[patent_no_of_claims] => 2
[patent_no_of_ind_claims] => 2
[patent_words_short_claim] => 155
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => patent
[pdf_file] => patents/04/696/04696810.pdf
[firstpage_image] =>[orig_patent_app_number] => 847148
[rel_patent_id] =>[rel_patent_doc_number] =>) 06/847148 | Wet process for the production of a readily sinterable powder material of perovskite or its solid solution | Apr 1, 1986 | Issued |