| Application number | Title of the application | Filing Date | Status |
|---|
Array
(
[id] => 2290437
[patent_doc_number] => 04710347
[patent_country] => US
[patent_kind] => NA
[patent_issue_date] => 1987-12-01
[patent_title] => 'Maraging steel having high strength and high toughness'
[patent_app_type] => 1
[patent_app_number] => 6/868594
[patent_app_country] => US
[patent_app_date] => 1986-05-30
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 3
[patent_figures_cnt] => 3
[patent_no_of_words] => 2307
[patent_no_of_claims] => 1
[patent_no_of_ind_claims] => 1
[patent_words_short_claim] => 41
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => patent
[pdf_file] => patents/04/710/04710347.pdf
[firstpage_image] =>[orig_patent_app_number] => 868594
[rel_patent_id] =>[rel_patent_doc_number] =>) 06/868594 | Maraging steel having high strength and high toughness | May 29, 1986 | Issued |
| 06/868104 | CLAD STEEL MATERIALS HAVING EXCELLENT DUCTILITY AND CORROSION RESISTANCE | May 28, 1986 | Abandoned |
| 06/866940 | METHOD OF MANUFACTURING NONMAGNETIC DRILLING STRING COMPONENTS | May 26, 1986 | Abandoned |
| 06/866220 | METHOD OF MANUFACTURING A COLD-ROLLED STEEL SHEET HAVING A GOOD DEEP DRAWABILITY | May 21, 1986 | Abandoned |
Array
(
[id] => 2312945
[patent_doc_number] => 04715908
[patent_country] => US
[patent_kind] => NA
[patent_issue_date] => 1987-12-29
[patent_title] => 'Duplex stainless steel product with improved mechanical properties'
[patent_app_type] => 1
[patent_app_number] => 6/864333
[patent_app_country] => US
[patent_app_date] => 1986-05-19
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 9
[patent_figures_cnt] => 9
[patent_no_of_words] => 3388
[patent_no_of_claims] => 1
[patent_no_of_ind_claims] => 1
[patent_words_short_claim] => 201
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => patent
[pdf_file] => patents/04/715/04715908.pdf
[firstpage_image] =>[orig_patent_app_number] => 864333
[rel_patent_id] =>[rel_patent_doc_number] =>) 06/864333 | Duplex stainless steel product with improved mechanical properties | May 18, 1986 | Issued |
Array
(
[id] => 2344255
[patent_doc_number] => 04703885
[patent_country] => US
[patent_kind] => NA
[patent_issue_date] => 1987-11-03
[patent_title] => 'Method of welding austenitic steel to ferritic steel with filler alloys'
[patent_app_type] => 1
[patent_app_number] => 6/862012
[patent_app_country] => US
[patent_app_date] => 1986-05-12
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 0
[patent_figures_cnt] => 0
[patent_no_of_words] => 3476
[patent_no_of_claims] => 3
[patent_no_of_ind_claims] => 1
[patent_words_short_claim] => 275
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => patent
[pdf_file] => patents/04/703/04703885.pdf
[firstpage_image] =>[orig_patent_app_number] => 862012
[rel_patent_id] =>[rel_patent_doc_number] =>) 06/862012 | Method of welding austenitic steel to ferritic steel with filler alloys | May 11, 1986 | Issued |
| 06/861419 | CHROMIUM CONTAINING ALLOY FOR FABRICATING PUNCH AND COUNTER PUNCH PLATES | May 8, 1986 | Abandoned |
| 06/856806 | DUPLEX STAINLESS STEEL SEAMLESS PIPE AND A METHOD FOR PRODUCING THE SAME | Apr 27, 1986 | Abandoned |
Array
(
[id] => 2551822
[patent_doc_number] => 04816217
[patent_country] => US
[patent_kind] => NA
[patent_issue_date] => 1989-03-28
[patent_title] => 'High-strength alloy for industrial vessels'
[patent_app_type] => 1
[patent_app_number] => 6/854340
[patent_app_country] => US
[patent_app_date] => 1986-04-21
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 1
[patent_figures_cnt] => 1
[patent_no_of_words] => 7032
[patent_no_of_claims] => 12
[patent_no_of_ind_claims] => 3
[patent_words_short_claim] => 94
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => patent
[pdf_file] => patents/04/816/04816217.pdf
[firstpage_image] =>[orig_patent_app_number] => 854340
[rel_patent_id] =>[rel_patent_doc_number] =>) 06/854340 | High-strength alloy for industrial vessels | Apr 20, 1986 | Issued |
Array
(
[id] => 2324082
[patent_doc_number] => 04705581
[patent_country] => US
[patent_kind] => NA
[patent_issue_date] => 1987-11-10
[patent_title] => 'Soft magnetic stainless steel'
[patent_app_type] => 1
[patent_app_number] => 6/851159
[patent_app_country] => US
[patent_app_date] => 1986-04-14
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 3
[patent_figures_cnt] => 5
[patent_no_of_words] => 3807
[patent_no_of_claims] => 3
[patent_no_of_ind_claims] => 3
[patent_words_short_claim] => 136
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => patent
[pdf_file] => patents/04/705/04705581.pdf
[firstpage_image] =>[orig_patent_app_number] => 851159
[rel_patent_id] =>[rel_patent_doc_number] =>) 06/851159 | Soft magnetic stainless steel | Apr 13, 1986 | Issued |
| 06/849569 | THERMALLY STABLE SUPER INVAR | Apr 7, 1986 | Abandoned |
| 06/850064 | ROLLED STEEL HAVING EXCELLENT RESISTANCE TO SULFIDE STRESS CORROSION CRACKING AND PROCESS FOR PRODUCING SAME | Apr 6, 1986 | Abandoned |
Array
(
[id] => 2481026
[patent_doc_number] => 04820486
[patent_country] => US
[patent_kind] => NA
[patent_issue_date] => 1989-04-11
[patent_title] => 'Low alloy steel having good stress corrosion cracking resistance'
[patent_app_type] => 1
[patent_app_number] => 6/846102
[patent_app_country] => US
[patent_app_date] => 1986-03-31
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 2
[patent_figures_cnt] => 2
[patent_no_of_words] => 6362
[patent_no_of_claims] => 2
[patent_no_of_ind_claims] => 2
[patent_words_short_claim] => 128
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => patent
[pdf_file] => patents/04/820/04820486.pdf
[firstpage_image] =>[orig_patent_app_number] => 846102
[rel_patent_id] =>[rel_patent_doc_number] =>) 06/846102 | Low alloy steel having good stress corrosion cracking resistance | Mar 30, 1986 | Issued |
Array
(
[id] => 2442466
[patent_doc_number] => 04721600
[patent_country] => US
[patent_kind] => NA
[patent_issue_date] => 1988-01-26
[patent_title] => 'Superplastic ferrous duplex-phase alloy and a hot working method therefor'
[patent_app_type] => 1
[patent_app_number] => 6/844661
[patent_app_country] => US
[patent_app_date] => 1986-03-27
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 2
[patent_figures_cnt] => 2
[patent_no_of_words] => 8810
[patent_no_of_claims] => 10
[patent_no_of_ind_claims] => 4
[patent_words_short_claim] => 182
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => patent
[pdf_file] => patents/04/721/04721600.pdf
[firstpage_image] =>[orig_patent_app_number] => 844661
[rel_patent_id] =>[rel_patent_doc_number] =>) 06/844661 | Superplastic ferrous duplex-phase alloy and a hot working method therefor | Mar 26, 1986 | Issued |
| 06/842914 | LAPPING TOOLS AND METHOD OF MANUFACTURING THE SAME | Mar 23, 1986 | Abandoned |
| 06/841291 | HIGH STRENGTH AND HIGH TOUGHNESS STEEL BAR, ROD AND WIRE AND THE PROCESS OF PRODUCING THE SAME | Mar 18, 1986 | Abandoned |
Array
(
[id] => 2440180
[patent_doc_number] => 04740255
[patent_country] => US
[patent_kind] => NA
[patent_issue_date] => 1988-04-26
[patent_title] => 'High strength weldable seamless tube of low alloy steel'
[patent_app_type] => 1
[patent_app_number] => 6/840064
[patent_app_country] => US
[patent_app_date] => 1986-03-17
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 3
[patent_figures_cnt] => 5
[patent_no_of_words] => 2904
[patent_no_of_claims] => 2
[patent_no_of_ind_claims] => 2
[patent_words_short_claim] => 171
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => patent
[pdf_file] => patents/04/740/04740255.pdf
[firstpage_image] =>[orig_patent_app_number] => 840064
[rel_patent_id] =>[rel_patent_doc_number] =>) 06/840064 | High strength weldable seamless tube of low alloy steel | Mar 16, 1986 | Issued |
Array
(
[id] => 2441962
[patent_doc_number] => 04755235
[patent_country] => US
[patent_kind] => NA
[patent_issue_date] => 1988-07-05
[patent_title] => 'Electrically conductive precipitation hardened copper alloy and a method for manufacturing the same'
[patent_app_type] => 1
[patent_app_number] => 6/840994
[patent_app_country] => US
[patent_app_date] => 1986-03-17
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 0
[patent_figures_cnt] => 0
[patent_no_of_words] => 2563
[patent_no_of_claims] => 16
[patent_no_of_ind_claims] => 3
[patent_words_short_claim] => 76
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => patent
[pdf_file] => patents/04/755/04755235.pdf
[firstpage_image] =>[orig_patent_app_number] => 840994
[rel_patent_id] =>[rel_patent_doc_number] =>) 06/840994 | Electrically conductive precipitation hardened copper alloy and a method for manufacturing the same | Mar 16, 1986 | Issued |
| 06/838378 | HIGH-STRENGTH HEAT-RESISTING FERRITIC STEEL PIPE AND TUBE | Mar 10, 1986 | Abandoned |
Array
(
[id] => 2323033
[patent_doc_number] => 04698103
[patent_country] => US
[patent_kind] => NA
[patent_issue_date] => 1987-10-06
[patent_title] => 'Method of manufacturing dual phase strip steel and steel strip manufactured by the method'
[patent_app_type] => 1
[patent_app_number] => 6/837195
[patent_app_country] => US
[patent_app_date] => 1986-03-10
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 4
[patent_figures_cnt] => 4
[patent_no_of_words] => 2413
[patent_no_of_claims] => 18
[patent_no_of_ind_claims] => 10
[patent_words_short_claim] => 28
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => patent
[pdf_file] => patents/04/698/04698103.pdf
[firstpage_image] =>[orig_patent_app_number] => 837195
[rel_patent_id] =>[rel_patent_doc_number] =>) 06/837195 | Method of manufacturing dual phase strip steel and steel strip manufactured by the method | Mar 9, 1986 | Issued |