Mark L. Shevin
Examiner (ID: 11241)
| Most Active Art Unit | 1793 |
| Art Unit(s) | 1793, 1733, 4116 |
| Total Applications | 254 |
| Issued Applications | 160 |
| Pending Applications | 1 |
| Abandoned Applications | 93 |
Applications
| Application number | Title of the application | Filing Date | Status |
|---|---|---|---|
Array
(
[id] => 5239647
[patent_doc_number] => 20070018138
[patent_country] => US
[patent_kind] => A1
[patent_issue_date] => 2007-01-25
[patent_title] => 'Highly pure hafnium material, target thin film comprising the same and method for producing highly pure hafnium'
[patent_app_type] => utility
[patent_app_number] => 10/565767
[patent_app_country] => US
[patent_app_date] => 2004-04-15
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 0
[patent_figures_cnt] => 0
[patent_no_of_words] => 2659
[patent_no_of_claims] => 21
[patent_no_of_ind_claims] => 3
[patent_words_short_claim] => 0
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => publication
[pdf_file] => publications/A1/0018/20070018138.pdf
[firstpage_image] =>[orig_patent_app_number] => 10565767
[rel_patent_id] =>[rel_patent_doc_number] =>) 10/565767 | Highly pure hafnium material, target thin film comprising the same and method for producing highly pure hafnium | Apr 14, 2004 | Issued |
Array
(
[id] => 5103743
[patent_doc_number] => 20070062618
[patent_country] => US
[patent_kind] => A1
[patent_issue_date] => 2007-03-22
[patent_title] => 'Aluminum alloy plate excellent in press formability and continuous resistance spot weldability and method for production thereof'
[patent_app_type] => utility
[patent_app_number] => 10/553316
[patent_app_country] => US
[patent_app_date] => 2004-04-13
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 0
[patent_figures_cnt] => 0
[patent_no_of_words] => 3817
[patent_no_of_claims] => 11
[patent_no_of_ind_claims] => 1
[patent_words_short_claim] => 0
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => publication
[pdf_file] => publications/A1/0062/20070062618.pdf
[firstpage_image] =>[orig_patent_app_number] => 10553316
[rel_patent_id] =>[rel_patent_doc_number] =>) 10/553316 | Aluminum alloy plate excellent in press formability and continuous resistance spot weldability and method for production thereof | Apr 12, 2004 | Abandoned |
Array
(
[id] => 5233310
[patent_doc_number] => 20070125465
[patent_country] => US
[patent_kind] => A1
[patent_issue_date] => 2007-06-07
[patent_title] => 'Planar, rolled semi-finished product of aluminum alloys'
[patent_app_type] => utility
[patent_app_number] => 10/551563
[patent_app_country] => US
[patent_app_date] => 2004-03-31
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 0
[patent_figures_cnt] => 0
[patent_no_of_words] => 1705
[patent_no_of_claims] => 4
[patent_no_of_ind_claims] => 2
[patent_words_short_claim] => 0
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => publication
[pdf_file] => publications/A1/0125/20070125465.pdf
[firstpage_image] =>[orig_patent_app_number] => 10551563
[rel_patent_id] =>[rel_patent_doc_number] =>) 10/551563 | Planar, rolled semi-finished product of aluminum alloys | Mar 30, 2004 | Issued |
Array
(
[id] => 5837556
[patent_doc_number] => 20060118214
[patent_country] => US
[patent_kind] => A1
[patent_issue_date] => 2006-06-08
[patent_title] => 'Method for producing aluminum alloy sheet material and an aluminium alloy sheet'
[patent_app_type] => utility
[patent_app_number] => 10/549673
[patent_app_country] => US
[patent_app_date] => 2004-03-19
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 4
[patent_figures_cnt] => 4
[patent_no_of_words] => 2050
[patent_no_of_claims] => 20
[patent_no_of_ind_claims] => 2
[patent_words_short_claim] => 0
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => publication
[pdf_file] => publications/A1/0118/20060118214.pdf
[firstpage_image] =>[orig_patent_app_number] => 10549673
[rel_patent_id] =>[rel_patent_doc_number] =>) 10/549673 | Method for producing aluminum alloy sheet material and an aluminium alloy sheet | Mar 18, 2004 | Issued |
Array
(
[id] => 5848784
[patent_doc_number] => 20060231975
[patent_country] => US
[patent_kind] => A1
[patent_issue_date] => 2006-10-19
[patent_title] => 'Method of producing metal mould cavities be means of ceramic and metal power sintering'
[patent_app_type] => utility
[patent_app_number] => 10/548220
[patent_app_country] => US
[patent_app_date] => 2004-03-01
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 3
[patent_figures_cnt] => 3
[patent_no_of_words] => 3499
[patent_no_of_claims] => 13
[patent_no_of_ind_claims] => 1
[patent_words_short_claim] => 0
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => publication
[pdf_file] => publications/A1/0231/20060231975.pdf
[firstpage_image] =>[orig_patent_app_number] => 10548220
[rel_patent_id] =>[rel_patent_doc_number] =>) 10/548220 | Method of producing metal mould cavities be means of ceramic and metal power sintering | Feb 29, 2004 | Abandoned |
Array
(
[id] => 322153
[patent_doc_number] => 07517383
[patent_country] => US
[patent_kind] => B2
[patent_issue_date] => 2009-04-14
[patent_title] => 'Method for recovery of zinc by countercurrent leaching'
[patent_app_type] => utility
[patent_app_number] => 10/544272
[patent_app_country] => US
[patent_app_date] => 2004-02-24
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 1
[patent_figures_cnt] => 1
[patent_no_of_words] => 3704
[patent_no_of_claims] => 12
[patent_no_of_ind_claims] => 1
[patent_words_short_claim] => 264
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => patent
[pdf_file] => patents/07/517/07517383.pdf
[firstpage_image] =>[orig_patent_app_number] => 10544272
[rel_patent_id] =>[rel_patent_doc_number] =>) 10/544272 | Method for recovery of zinc by countercurrent leaching | Feb 23, 2004 | Issued |
Array
(
[id] => 5810205
[patent_doc_number] => 20060081313
[patent_country] => US
[patent_kind] => A1
[patent_issue_date] => 2006-04-20
[patent_title] => 'Method for the production of a semi-finished product made of zirconium alloy for the production of a flat product and use thereof'
[patent_app_type] => utility
[patent_app_number] => 10/541262
[patent_app_country] => US
[patent_app_date] => 2004-01-09
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 3
[patent_figures_cnt] => 3
[patent_no_of_words] => 3098
[patent_no_of_claims] => 6
[patent_no_of_ind_claims] => 2
[patent_words_short_claim] => 0
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => publication
[pdf_file] => publications/A1/0081/20060081313.pdf
[firstpage_image] =>[orig_patent_app_number] => 10541262
[rel_patent_id] =>[rel_patent_doc_number] =>) 10/541262 | Method for the production of a semi-finished product made of zirconium alloy for the production of a flat product and use thereof | Jan 8, 2004 | Abandoned |
Array
(
[id] => 62034
[patent_doc_number] => 07763132
[patent_country] => US
[patent_kind] => B2
[patent_issue_date] => 2010-07-27
[patent_title] => 'Method of producing a zirconium alloy semi-finished product for the production of elongated product and use thereof'
[patent_app_type] => utility
[patent_app_number] => 10/541774
[patent_app_country] => US
[patent_app_date] => 2004-01-07
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 1
[patent_figures_cnt] => 1
[patent_no_of_words] => 3071
[patent_no_of_claims] => 10
[patent_no_of_ind_claims] => 2
[patent_words_short_claim] => 51
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => patent
[pdf_file] => patents/07/763/07763132.pdf
[firstpage_image] =>[orig_patent_app_number] => 10541774
[rel_patent_id] =>[rel_patent_doc_number] =>) 10/541774 | Method of producing a zirconium alloy semi-finished product for the production of elongated product and use thereof | Jan 6, 2004 | Issued |
Array
(
[id] => 5726659
[patent_doc_number] => 20060057419
[patent_country] => US
[patent_kind] => A1
[patent_issue_date] => 2006-03-16
[patent_title] => 'High-strength steel product excelling in fatigue strength and process for producing the same'
[patent_app_type] => utility
[patent_app_number] => 10/530134
[patent_app_country] => US
[patent_app_date] => 2004-01-07
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 0
[patent_figures_cnt] => 0
[patent_no_of_words] => 7088
[patent_no_of_claims] => 16
[patent_no_of_ind_claims] => 2
[patent_words_short_claim] => 0
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => publication
[pdf_file] => publications/A1/0057/20060057419.pdf
[firstpage_image] =>[orig_patent_app_number] => 10530134
[rel_patent_id] =>[rel_patent_doc_number] =>) 10/530134 | High-strength steel product excelling in fatigue strength and process for producing the same | Jan 6, 2004 | Abandoned |
Array
(
[id] => 5732550
[patent_doc_number] => 20060257667
[patent_country] => US
[patent_kind] => A1
[patent_issue_date] => 2006-11-16
[patent_title] => 'Composition for forming silicon-aluminum film, silicon-aluminum film and method for forming the same'
[patent_app_type] => utility
[patent_app_number] => 10/542358
[patent_app_country] => US
[patent_app_date] => 2003-12-24
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 2
[patent_figures_cnt] => 2
[patent_no_of_words] => 7368
[patent_no_of_claims] => 5
[patent_no_of_ind_claims] => 1
[patent_words_short_claim] => 0
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => publication
[pdf_file] => publications/A1/0257/20060257667.pdf
[firstpage_image] =>[orig_patent_app_number] => 10542358
[rel_patent_id] =>[rel_patent_doc_number] =>) 10/542358 | Composition for forming silicon-aluminum film, silicon-aluminum film and method for forming the same | Dec 23, 2003 | Abandoned |
Array
(
[id] => 5867882
[patent_doc_number] => 20060162499
[patent_country] => US
[patent_kind] => A1
[patent_issue_date] => 2006-07-27
[patent_title] => 'Apparatus for manufacturing molten irons by hot compacting fine direct reduced irons and calcined additives and method using the same'
[patent_app_type] => utility
[patent_app_number] => 10/539743
[patent_app_country] => US
[patent_app_date] => 2003-12-19
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 10
[patent_figures_cnt] => 10
[patent_no_of_words] => 8386
[patent_no_of_claims] => 30
[patent_no_of_ind_claims] => 3
[patent_words_short_claim] => 0
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => publication
[pdf_file] => publications/A1/0162/20060162499.pdf
[firstpage_image] =>[orig_patent_app_number] => 10539743
[rel_patent_id] =>[rel_patent_doc_number] =>) 10/539743 | Apparatus for manufacturing molten irons by hot compacting fine direct reduced irons and calcined additives and method using the same | Dec 18, 2003 | Issued |
Array
(
[id] => 201532
[patent_doc_number] => 07632334
[patent_country] => US
[patent_kind] => B2
[patent_issue_date] => 2009-12-15
[patent_title] => 'Method and plant for the heat treatment of solids containing iron oxide'
[patent_app_type] => utility
[patent_app_number] => 10/540434
[patent_app_country] => US
[patent_app_date] => 2003-12-12
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 2
[patent_figures_cnt] => 2
[patent_no_of_words] => 4254
[patent_no_of_claims] => 10
[patent_no_of_ind_claims] => 1
[patent_words_short_claim] => 206
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => patent
[pdf_file] => patents/07/632/07632334.pdf
[firstpage_image] =>[orig_patent_app_number] => 10540434
[rel_patent_id] =>[rel_patent_doc_number] =>) 10/540434 | Method and plant for the heat treatment of solids containing iron oxide | Dec 11, 2003 | Issued |
Array
(
[id] => 181613
[patent_doc_number] => 07651547
[patent_country] => US
[patent_kind] => B2
[patent_issue_date] => 2010-01-26
[patent_title] => 'Fluidized bed method and plant for the heat treatment of solids containing titanium'
[patent_app_type] => utility
[patent_app_number] => 10/540376
[patent_app_country] => US
[patent_app_date] => 2003-12-10
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 3
[patent_figures_cnt] => 3
[patent_no_of_words] => 7299
[patent_no_of_claims] => 27
[patent_no_of_ind_claims] => 1
[patent_words_short_claim] => 194
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => patent
[pdf_file] => patents/07/651/07651547.pdf
[firstpage_image] =>[orig_patent_app_number] => 10540376
[rel_patent_id] =>[rel_patent_doc_number] =>) 10/540376 | Fluidized bed method and plant for the heat treatment of solids containing titanium | Dec 9, 2003 | Issued |
Array
(
[id] => 5846379
[patent_doc_number] => 20060230879
[patent_country] => US
[patent_kind] => A1
[patent_issue_date] => 2006-10-19
[patent_title] => 'Method and plant for the heat treatment of sulfidic ores using annular fluidized'
[patent_app_type] => utility
[patent_app_number] => 10/540352
[patent_app_country] => US
[patent_app_date] => 2003-12-10
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 2
[patent_figures_cnt] => 2
[patent_no_of_words] => 5939
[patent_no_of_claims] => 35
[patent_no_of_ind_claims] => 1
[patent_words_short_claim] => 0
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => publication
[pdf_file] => publications/A1/0230/20060230879.pdf
[firstpage_image] =>[orig_patent_app_number] => 10540352
[rel_patent_id] =>[rel_patent_doc_number] =>) 10/540352 | Method and plant for the heat treatment of sulfidic ores using annular fluidized | Dec 9, 2003 | Abandoned |
Array
(
[id] => 239195
[patent_doc_number] => 07591910
[patent_country] => US
[patent_kind] => B2
[patent_issue_date] => 2009-09-22
[patent_title] => 'Bulk amorphous refractory glasses based on the Ni(-Cu-)-Ti(-Zr)-Al alloy system'
[patent_app_type] => utility
[patent_app_number] => 10/535317
[patent_app_country] => US
[patent_app_date] => 2003-12-04
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 2
[patent_figures_cnt] => 2
[patent_no_of_words] => 5518
[patent_no_of_claims] => 15
[patent_no_of_ind_claims] => 2
[patent_words_short_claim] => 33
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => patent
[pdf_file] => patents/07/591/07591910.pdf
[firstpage_image] =>[orig_patent_app_number] => 10535317
[rel_patent_id] =>[rel_patent_doc_number] =>) 10/535317 | Bulk amorphous refractory glasses based on the Ni(-Cu-)-Ti(-Zr)-Al alloy system | Dec 3, 2003 | Issued |
Array
(
[id] => 209630
[patent_doc_number] => 07625422
[patent_country] => US
[patent_kind] => B2
[patent_issue_date] => 2009-12-01
[patent_title] => 'Method and plant for the heat treatment of solids containing iron oxide using a fluidized bed reactor'
[patent_app_type] => utility
[patent_app_number] => 10/540435
[patent_app_country] => US
[patent_app_date] => 2003-12-01
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 3
[patent_figures_cnt] => 3
[patent_no_of_words] => 7130
[patent_no_of_claims] => 18
[patent_no_of_ind_claims] => 1
[patent_words_short_claim] => 209
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => patent
[pdf_file] => patents/07/625/07625422.pdf
[firstpage_image] =>[orig_patent_app_number] => 10540435
[rel_patent_id] =>[rel_patent_doc_number] =>) 10/540435 | Method and plant for the heat treatment of solids containing iron oxide using a fluidized bed reactor | Nov 30, 2003 | Issued |
Array
(
[id] => 4562950
[patent_doc_number] => 07857918
[patent_country] => US
[patent_kind] => B2
[patent_issue_date] => 2010-12-28
[patent_title] => 'Method of production of steel product with nanocrystallized surface layer'
[patent_app_type] => utility
[patent_app_number] => 10/535346
[patent_app_country] => US
[patent_app_date] => 2003-11-17
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 2
[patent_figures_cnt] => 4
[patent_no_of_words] => 4909
[patent_no_of_claims] => 17
[patent_no_of_ind_claims] => 2
[patent_words_short_claim] => 105
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => patent
[pdf_file] => patents/07/857/07857918.pdf
[firstpage_image] =>[orig_patent_app_number] => 10535346
[rel_patent_id] =>[rel_patent_doc_number] =>) 10/535346 | Method of production of steel product with nanocrystallized surface layer | Nov 16, 2003 | Issued |
Array
(
[id] => 5572013
[patent_doc_number] => 20090139372
[patent_country] => US
[patent_kind] => A1
[patent_issue_date] => 2009-06-04
[patent_title] => 'Production method of pure metal/alloy super-micro powder'
[patent_app_type] => utility
[patent_app_number] => 10/578298
[patent_app_country] => US
[patent_app_date] => 2003-11-05
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 3
[patent_figures_cnt] => 3
[patent_no_of_words] => 4761
[patent_no_of_claims] => 8
[patent_no_of_ind_claims] => 2
[patent_words_short_claim] => 0
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => publication
[pdf_file] => publications/A1/0139/20090139372.pdf
[firstpage_image] =>[orig_patent_app_number] => 10578298
[rel_patent_id] =>[rel_patent_doc_number] =>) 10/578298 | Production method of pure metal/alloy super-micro powder | Nov 4, 2003 | Issued |
Array
(
[id] => 5652042
[patent_doc_number] => 20060137777
[patent_country] => US
[patent_kind] => A1
[patent_issue_date] => 2006-06-29
[patent_title] => 'Method of increasing toughness of heat-affected part of steel product welded joint'
[patent_app_type] => utility
[patent_app_number] => 10/533607
[patent_app_country] => US
[patent_app_date] => 2003-10-29
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 4
[patent_figures_cnt] => 4
[patent_no_of_words] => 5978
[patent_no_of_claims] => 5
[patent_no_of_ind_claims] => 4
[patent_words_short_claim] => 0
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => publication
[pdf_file] => publications/A1/0137/20060137777.pdf
[firstpage_image] =>[orig_patent_app_number] => 10533607
[rel_patent_id] =>[rel_patent_doc_number] =>) 10/533607 | Method of improvement of toughness of heat affected zone at welded joint of steel plate | Oct 28, 2003 | Issued |
Array
(
[id] => 7108192
[patent_doc_number] => 20050205645
[patent_country] => US
[patent_kind] => A1
[patent_issue_date] => 2005-09-22
[patent_title] => 'Refined aluminium strip or sheet for electrolytic capacitors'
[patent_app_type] => utility
[patent_app_number] => 10/524118
[patent_app_country] => US
[patent_app_date] => 2003-09-22
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 0
[patent_figures_cnt] => 0
[patent_no_of_words] => 2099
[patent_no_of_claims] => 4
[patent_no_of_ind_claims] => 1
[patent_words_short_claim] => 0
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => publication
[pdf_file] => publications/A1/0205/20050205645.pdf
[firstpage_image] =>[orig_patent_app_number] => 10524118