Application number | Title of the application | Filing Date | Status |
---|
Array
(
[id] => 3693015
[patent_doc_number] => 05618635
[patent_country] => US
[patent_kind] => NA
[patent_issue_date] => 1997-04-08
[patent_title] => 'Macrocomposite bodies'
[patent_app_type] => 1
[patent_app_number] => 8/411055
[patent_app_country] => US
[patent_app_date] => 1995-03-27
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 3
[patent_figures_cnt] => 13
[patent_no_of_words] => 17146
[patent_no_of_claims] => 9
[patent_no_of_ind_claims] => 2
[patent_words_short_claim] => 133
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => patent
[pdf_file] => patents/05/618/05618635.pdf
[firstpage_image] =>[orig_patent_app_number] => 411055
[rel_patent_id] =>[rel_patent_doc_number] =>) 08/411055 | Macrocomposite bodies | Mar 26, 1995 | Issued |
Array
(
[id] => 4031543
[patent_doc_number] => 05856025
[patent_country] => US
[patent_kind] => NA
[patent_issue_date] => 1999-01-05
[patent_title] => 'Metal matrix composites'
[patent_app_type] => 1
[patent_app_number] => 8/399306
[patent_app_country] => US
[patent_app_date] => 1995-03-06
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 2
[patent_figures_cnt] => 3
[patent_no_of_words] => 7638
[patent_no_of_claims] => 16
[patent_no_of_ind_claims] => 5
[patent_words_short_claim] => 71
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => patent
[pdf_file] => patents/05/856/05856025.pdf
[firstpage_image] =>[orig_patent_app_number] => 399306
[rel_patent_id] =>[rel_patent_doc_number] =>) 08/399306 | Metal matrix composites | Mar 5, 1995 | Issued |
Array
(
[id] => 3492746
[patent_doc_number] => 05531977
[patent_country] => US
[patent_kind] => NA
[patent_issue_date] => 1996-07-02
[patent_title] => 'Process for producing acicular .gamma.-FeOOH particles'
[patent_app_type] => 1
[patent_app_number] => 8/400004
[patent_app_country] => US
[patent_app_date] => 1995-03-06
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 1
[patent_figures_cnt] => 1
[patent_no_of_words] => 4498
[patent_no_of_claims] => 10
[patent_no_of_ind_claims] => 1
[patent_words_short_claim] => 102
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => patent
[pdf_file] => patents/05/531/05531977.pdf
[firstpage_image] =>[orig_patent_app_number] => 400004
[rel_patent_id] =>[rel_patent_doc_number] =>) 08/400004 | Process for producing acicular .gamma.-FeOOH particles | Mar 5, 1995 | Issued |
Array
(
[id] => 3872287
[patent_doc_number] => 05747178
[patent_country] => US
[patent_kind] => NA
[patent_issue_date] => 1998-05-05
[patent_title] => 'Deposition of silver layer on nonconducting substrate'
[patent_app_type] => 1
[patent_app_number] => 8/399281
[patent_app_country] => US
[patent_app_date] => 1995-03-06
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 0
[patent_figures_cnt] => 0
[patent_no_of_words] => 5134
[patent_no_of_claims] => 35
[patent_no_of_ind_claims] => 5
[patent_words_short_claim] => 76
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => patent
[pdf_file] => patents/05/747/05747178.pdf
[firstpage_image] =>[orig_patent_app_number] => 399281
[rel_patent_id] =>[rel_patent_doc_number] =>) 08/399281 | Deposition of silver layer on nonconducting substrate | Mar 5, 1995 | Issued |
Array
(
[id] => 3508339
[patent_doc_number] => 05587248
[patent_country] => US
[patent_kind] => NA
[patent_issue_date] => 1996-12-24
[patent_title] => 'Corrosion resistant nickel plating steel sheet or strip and manufacturing method thereof'
[patent_app_type] => 1
[patent_app_number] => 8/400387
[patent_app_country] => US
[patent_app_date] => 1995-03-03
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 1
[patent_figures_cnt] => 1
[patent_no_of_words] => 4931
[patent_no_of_claims] => 3
[patent_no_of_ind_claims] => 1
[patent_words_short_claim] => 162
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => patent
[pdf_file] => patents/05/587/05587248.pdf
[firstpage_image] =>[orig_patent_app_number] => 400387
[rel_patent_id] =>[rel_patent_doc_number] =>) 08/400387 | Corrosion resistant nickel plating steel sheet or strip and manufacturing method thereof | Mar 2, 1995 | Issued |
08/392846 | PROCESS FOR MANUFACTURING HIGH PURITY NICKEL CHLORIDE BY RECYCLING WASTE NICKEL ANODE | Feb 28, 1995 | Abandoned |
08/395657 | DEHYDRATION OF FLUORIDE MIXTURES | Feb 27, 1995 | Abandoned |
08/396009 | METHOD FOR RECYCLING METHYL BROMIDE | Feb 27, 1995 | Abandoned |
08/392618 | INNER-SHIELD MATERIAL TO BE ATTACHED INSIDE A COLOR CATHODE RAY TUBE AND MANUFACTURING METHOD THEREOF | Feb 21, 1995 | Abandoned |
Array
(
[id] => 3664168
[patent_doc_number] => 05599633
[patent_country] => US
[patent_kind] => NA
[patent_issue_date] => 1997-02-04
[patent_title] => 'Wire electrode for electro-discharge machining'
[patent_app_type] => 1
[patent_app_number] => 8/390417
[patent_app_country] => US
[patent_app_date] => 1995-02-17
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 1
[patent_figures_cnt] => 1
[patent_no_of_words] => 2101
[patent_no_of_claims] => 11
[patent_no_of_ind_claims] => 1
[patent_words_short_claim] => 105
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => patent
[pdf_file] => patents/05/599/05599633.pdf
[firstpage_image] =>[orig_patent_app_number] => 390417
[rel_patent_id] =>[rel_patent_doc_number] =>) 08/390417 | Wire electrode for electro-discharge machining | Feb 16, 1995 | Issued |
Array
(
[id] => 3551343
[patent_doc_number] => 05543130
[patent_country] => US
[patent_kind] => NA
[patent_issue_date] => 1996-08-06
[patent_title] => 'Metal ceramic composite structure'
[patent_app_type] => 1
[patent_app_number] => 8/387390
[patent_app_country] => US
[patent_app_date] => 1995-02-13
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 7
[patent_figures_cnt] => 15
[patent_no_of_words] => 6855
[patent_no_of_claims] => 3
[patent_no_of_ind_claims] => 1
[patent_words_short_claim] => 182
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => patent
[pdf_file] => patents/05/543/05543130.pdf
[firstpage_image] =>[orig_patent_app_number] => 387390
[rel_patent_id] =>[rel_patent_doc_number] =>) 08/387390 | Metal ceramic composite structure | Feb 12, 1995 | Issued |
Array
(
[id] => 3619386
[patent_doc_number] => 05612013
[patent_country] => US
[patent_kind] => NA
[patent_issue_date] => 1997-03-18
[patent_title] => 'Method for synthesis of borazine'
[patent_app_type] => 1
[patent_app_number] => 8/386930
[patent_app_country] => US
[patent_app_date] => 1995-02-10
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 0
[patent_figures_cnt] => 0
[patent_no_of_words] => 1784
[patent_no_of_claims] => 19
[patent_no_of_ind_claims] => 3
[patent_words_short_claim] => 69
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => patent
[pdf_file] => patents/05/612/05612013.pdf
[firstpage_image] =>[orig_patent_app_number] => 386930
[rel_patent_id] =>[rel_patent_doc_number] =>) 08/386930 | Method for synthesis of borazine | Feb 9, 1995 | Issued |
Array
(
[id] => 3579128
[patent_doc_number] => 05580668
[patent_country] => US
[patent_kind] => NA
[patent_issue_date] => 1996-12-03
[patent_title] => 'Aluminum-palladium alloy for initiation of electroless plating'
[patent_app_type] => 1
[patent_app_number] => 8/371929
[patent_app_country] => US
[patent_app_date] => 1995-01-12
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 5
[patent_figures_cnt] => 11
[patent_no_of_words] => 6865
[patent_no_of_claims] => 17
[patent_no_of_ind_claims] => 2
[patent_words_short_claim] => 156
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => patent
[pdf_file] => patents/05/580/05580668.pdf
[firstpage_image] =>[orig_patent_app_number] => 371929
[rel_patent_id] =>[rel_patent_doc_number] =>) 08/371929 | Aluminum-palladium alloy for initiation of electroless plating | Jan 11, 1995 | Issued |
08/370749 | METHOD FOR MAKING COPPER (I) OXIDE POWDERS BY AEROSOL DECOMPOSITION | Jan 9, 1995 | Abandoned |
Array
(
[id] => 4390315
[patent_doc_number] => 06296826
[patent_country] => US
[patent_kind] => NA
[patent_issue_date] => 2001-10-02
[patent_title] => 'Method for the preparation of vitrified silica particles'
[patent_app_type] => 1
[patent_app_number] => 8/366762
[patent_app_country] => US
[patent_app_date] => 1994-12-30
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 0
[patent_figures_cnt] => 0
[patent_no_of_words] => 4793
[patent_no_of_claims] => 3
[patent_no_of_ind_claims] => 1
[patent_words_short_claim] => 221
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => patent
[pdf_file] => patents/06/296/06296826.pdf
[firstpage_image] =>[orig_patent_app_number] => 366762
[rel_patent_id] =>[rel_patent_doc_number] =>) 08/366762 | Method for the preparation of vitrified silica particles | Dec 29, 1994 | Issued |
Array
(
[id] => 3501132
[patent_doc_number] => 05514359
[patent_country] => US
[patent_kind] => NA
[patent_issue_date] => 1996-05-07
[patent_title] => 'Process for making anhydrous magnesium chloride'
[patent_app_type] => 1
[patent_app_number] => 8/359857
[patent_app_country] => US
[patent_app_date] => 1994-12-20
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 3
[patent_figures_cnt] => 3
[patent_no_of_words] => 5207
[patent_no_of_claims] => 18
[patent_no_of_ind_claims] => 2
[patent_words_short_claim] => 105
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => patent
[pdf_file] => patents/05/514/05514359.pdf
[firstpage_image] =>[orig_patent_app_number] => 359857
[rel_patent_id] =>[rel_patent_doc_number] =>) 08/359857 | Process for making anhydrous magnesium chloride | Dec 19, 1994 | Issued |
Array
(
[id] => 1526915
[patent_doc_number] => 06478828
[patent_country] => US
[patent_kind] => B1
[patent_issue_date] => 2002-11-12
[patent_title] => 'Process for the crystallization of an inorganic substance'
[patent_app_type] => B1
[patent_app_number] => 08/358974
[patent_app_country] => US
[patent_app_date] => 1994-12-19
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 4
[patent_figures_cnt] => 4
[patent_no_of_words] => 3470
[patent_no_of_claims] => 14
[patent_no_of_ind_claims] => 3
[patent_words_short_claim] => 163
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => patent
[pdf_file] => patents/06/478/06478828.pdf
[firstpage_image] =>[orig_patent_app_number] => 08358974
[rel_patent_id] =>[rel_patent_doc_number] =>) 08/358974 | Process for the crystallization of an inorganic substance | Dec 18, 1994 | Issued |
Array
(
[id] => 3662443
[patent_doc_number] => 05599518
[patent_country] => US
[patent_kind] => NA
[patent_issue_date] => 1997-02-04
[patent_title] => 'Catalytic process for chlorine dioxide generation from chloric acid'
[patent_app_type] => 1
[patent_app_number] => 8/348012
[patent_app_country] => US
[patent_app_date] => 1994-12-01
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 2
[patent_figures_cnt] => 2
[patent_no_of_words] => 6876
[patent_no_of_claims] => 15
[patent_no_of_ind_claims] => 1
[patent_words_short_claim] => 160
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => patent
[pdf_file] => patents/05/599/05599518.pdf
[firstpage_image] =>[orig_patent_app_number] => 348012
[rel_patent_id] =>[rel_patent_doc_number] =>) 08/348012 | Catalytic process for chlorine dioxide generation from chloric acid | Nov 30, 1994 | Issued |
Array
(
[id] => 3417705
[patent_doc_number] => 05478660
[patent_country] => US
[patent_kind] => NA
[patent_issue_date] => 1995-12-26
[patent_title] => 'Article having a decorative and protective coating simulating brass'
[patent_app_type] => 1
[patent_app_number] => 8/346807
[patent_app_country] => US
[patent_app_date] => 1994-11-30
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 1
[patent_figures_cnt] => 1
[patent_no_of_words] => 3356
[patent_no_of_claims] => 36
[patent_no_of_ind_claims] => 4
[patent_words_short_claim] => 59
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => patent
[pdf_file] => patents/05/478/05478660.pdf
[firstpage_image] =>[orig_patent_app_number] => 346807
[rel_patent_id] =>[rel_patent_doc_number] =>) 08/346807 | Article having a decorative and protective coating simulating brass | Nov 29, 1994 | Issued |
Array
(
[id] => 3563523
[patent_doc_number] => 05482788
[patent_country] => US
[patent_kind] => NA
[patent_issue_date] => 1996-01-09
[patent_title] => 'Article having a protective coating simulating brass'
[patent_app_type] => 1
[patent_app_number] => 8/346801
[patent_app_country] => US
[patent_app_date] => 1994-11-30
[patent_effective_date] => 0000-00-00
[patent_drawing_sheets_cnt] => 1
[patent_figures_cnt] => 1
[patent_no_of_words] => 2755
[patent_no_of_claims] => 19
[patent_no_of_ind_claims] => 4
[patent_words_short_claim] => 51
[patent_maintenance] => 1
[patent_no_of_assignments] => 0
[patent_current_assignee] =>[type] => patent
[pdf_file] => patents/05/482/05482788.pdf
[firstpage_image] =>[orig_patent_app_number] => 346801